321 Stainless Steel Coil
321 Stainless Steel Coil
321 Stainless Steel Coil
321 Stainless Steel Coil

321 Stainless Steel Coil

321 stainless steel coil is a free-machining austenitic chromium-nickel austenitic alloy (18% Cr, 12% Ni) that provides good corrosion resistance in a wide range of corrosive environments.

321 stainless steel coils are widely used in the chemical and petrochemical industries where its corrosion resistance properties can be put to good use. The alloy also finds application in marine environments where chloride stress corrosion cracking must be avoided. It is also used for food processing equipment such as food blenders and mixers, beverage dispensing equipment and heat exchangers.


321 Stainless Steel Coil Specifications

HardnessSoft, Hard, Half Hard, Quarter Hard, Spring Hard as customer’s requirements
Thickness0.02mm-6.0mm
Width1.0mm-1500mm
EdgeSlit/Mill
Quantity Tolerance±10%
Paper Core Internal DiameterØ500mm paper core, special internal diameter core and without paper core on customer request
Surface FinishNO.1/2B/2D/BA/HL/Brushed/6K/8K Mirror,etc
PackagingWooden Pallet/Wooden Case
SampleThe sample of 321 stainless steel coil is available


Chemical Compositions

GradeStandardCSiMnPSCrNiMo
321ASTM A240≤0.08≤1.00≤2.00≤0.045≤0.03017.00-19.009.00-12.00


Mechanical Properties

GradeEN GradeYield Strength Rp0.2(N/mm²)Tensile Strength Rm(N/mm²)HardnessVickers Hardness(HV)Elongation A50%
3211.4541≥205≥520Annealed≤200≥40


surfaces.jpg

Properties of 321 stainless steel
Ni-Cr-Mo-type austenitic stainless steel, its performance with a 304 stainless steel plate is very similar, but due to the addition of titanium, it has a better intergranular corrosion resistance and high temperature strength. The addition of titanium to make it effective control of the formation of chromium carbide .

321 stainless steel with Ti as a stabilizing element exists, but it is the creep strength of steel at high temperatures much better than 316L.

321 stainless steel

Standard

Grade

Chemical Composition %

Temper

Yied strength/Mpa

Tensile strength/Mpa

Elongation %

Hardness

GB

1Cr18Ni9Ti

C≤0.08,Mn≤2.00,Si≤0.75,P≤0.045,S≤0.0.30,Cr 17.0~19.0,Ni 9.0~12.0,N≤0.10,Ti〔5x﹙C+N﹚〕~0.70

hot /cold rolled

≥205

≥518

≥40

HV≤200

USA

321

JIS

SUS321

German

1.4541

321 :high inter-granular corrosion resistance of chemical, coal, oil field open machine, heat treatment difficulties of building heat-resistant parts.
  • 1.Oil and gas burning pipeline

  • 2.Engine exhaust pipe

  • 3.Shell of the boiler, heat exchangers, heating furnace part

  • 4.Silencer for diesel parts

  • 5.Boilers and pressure vessels

  • 6.Chemical transportation vehicle

  • 7.Expansion joint

  • 8.Furnace pipes and drying machines for spiral welded pipe

Package Information:JQ Metal are packed and labeled according to the regulations and customer's requests. Great care is taken to avoid any damage which might otherwise be caused during storage or transportation. In addition, clear labels are tagged on the outside of the packages for easy identification of the product I. D. and quality information.

Contact Us

We don't use cookies to personalize content and analyze our traffic. We only contact you through the form and email.
Privacy Policy
×